Semiconductor Fabrication Basics – Home Chip Lab

A brief introduction to semiconductor fabrication processes and terminology. It is not intended to be an in depth view of any single process, but rather an overview so that provides enough information for someone to get started with making diodes and transistors at home.

Tour of my home chip fab setup in early 2017. I’ve been accumulating this equipment since October of 2016.

 

 

Step by step FET fabrication

 

High vacuum basics